Gentlemen,
Has any one out any experience this product? 500 to 1500 degrees! One review stated it still flaked after some amount of time.
I have a bead blaster in my garage, so can get older headers pretty clean. Use rubber gloves so no finger oils, residual solvents, etc.
Tend to flash fresh metal with cheap spray clear coat to keep surface rust at bay, here in the humid South.
Looking to coat a new set of Hookers for the 440 and coat two older small block pairs. All input is welcomed.